Izingcaphuno ezisheshayo nezihle kakhulu, abeluleki abanolwazi ukukusiza ukuthi ukhethe umkhiqizo olungile ovumelana nazo zonke izidingo zakho, isikhathi esifushane sokukhiqiza, ukuphathwa kwekhwalithi ephezulu okunomthwalo wemfanelo kanye nezinsizakalo ezihlukile zokukhokha nezokuthumela izindaba zeNeedle 450 Tissue E-Glass Fiberglass Mat Roll Stitched, We sithumele emazweni nasezifundeni ezingaphezu kuka-40, ezithole ukuthandwa okuphezulu kubathengi bethu yonke indawo emhlabeni jikelele.
Izingcaphuno ezisheshayo nezihle kakhulu, abeluleki abanolwazi ukukusiza ukhethe umkhiqizo olungile ovumelana nazo zonke izidingo zakho, isikhathi esifushane sokukhiqiza, ukuphathwa kwekhwalithi ephezulu okunomthwalo wemfanelo kanye nezinsizakalo ezihlukile zokukhokha kanye nezindaba zokuthumelaChina Fiberglass Mat kanye Fiberglass oqoshiwe strand mat, Eminyakeni engu-11, siye sabamba iqhaza emibukisweni engaphezu kuka-20, sithola ukunconywa okuphezulu kakhulu kukhasimende ngalinye. Inkampani yethu ihlale ihlose ukuletha ikhasimende imikhiqizo ehamba phambili ngentengo ephansi. Besenza imizamo emikhulu yokufeza lesi simo esiwinayo futhi sikwamukela ngobuqotho ukuthi uhlanganyele nathi. Hlanganyela nathi, ubonise ubuhle bakho. Sizohlala siyisinqumo sakho sokuqala. Sithembe, awusoze waphelelwa yinhliziyo.
1. Ukubeka izandla: Ukubeka izandla kuyindlela eyinhloko yokukhiqiza i-FRP. Omata bemicu abaqoshwe nge-fiberglass, omata abaqhubekayo, nomata abathungiwe konke kungasetshenziswa ezindaweni zokubeka izandla. Ukusetshenziswa kwe-aumata oboshwe ngomthungoinganciphisa inani lezendlalelo futhi ithuthukise ukusebenza kahle kwemisebenzi yokubeka izandla. Nokho, ngenxa yokuthi umata oboshiwe unemicu eyengeziwe yamakhemikhali e-fiber stitchbonding, amabhamuza akulula ukuwaxosha, imikhiqizo ye-fiberglass inamabhamuza amaningi amise okwenaliti, futhi ingaphezulu lizwakala limahhadlahhadla futhi lingasheleli. Ukwengeza, umata othungiwe uyindwangu esindayo, futhi ukumbozwa kwesikhunta kufushane kunalowo we-cut cut kanye ne-mat eqhubekayo. Lapho wenza imikhiqizo enezimo eziyinkimbinkimbi, kulula ukwenza ama-voids ekujikeni. Inqubo yokubeka isandla idinga ukuthi umata ube nezici zezinga lokungena ngokushesha kweresin, ukuqedwa kalula kwamabhamuza omoya, nokumbozwa kahle kwesikhunta.
2. I-pultrusion: Inqubo ye-pultrusion ingenye yezindlela eziyinhloko ezisetshenziswayo zokuzizwa okuqhubekayo kanyeamacansi athungiwe. Ngokuvamile, isetshenziswa ngokuhambisana nokuzulazula okungasontekile. Ukusebenzisaumata oqhubekayokanye nomata othungiwe njengemikhiqizo ephuhliwe kungathuthukisa kakhulu i-hoop namandla aguquguqukayo emikhiqizo futhi kuvimbele imikhiqizo ukuthi ingaqhekeki. Inqubo ye-pultrusion idinga ukuthi i-mat ibe nokusatshalaliswa kwefayibha elinganayo, amandla aqine kakhulu, izinga lokungena ngokushesha kwe-resin, ukuguquguquka okuhle nokugcwaliswa kwesikhunta, futhi umata kufanele ube nobude obuthile obuqhubekayo.
I-3.RTM: Ukubunjwa kokudluliselwa kwe-resin (RTM) kuyinqubo yokubumba evaliwe. Yakhiwe ngama-half-moulds amabili, isikhunta sesifazane kanye nesikhunta sowesilisa, ipompo elicindezelayo kanye nesibhamu somjovo, ngaphandle komshini wokunyathelisa. Inqubo ye-RTM ivamise ukusebenzisa omati abaqhubekayo nababoshiwe kunemicu eqoshiwe. Ishidi le-mat liyadingeka ukuthi libe nezici ukuthi ishidi le-mat kufanele ligcwaliswe kalula nge-resin, ukungena komoya okuhle, ukumelana okuhle kwe-resin scour kanye nokuguquguquka okuhle kakhulu.
4.Inqubo yokuvala:amacansi ama-strand aqoshiwefuthi amacansi aqhubekayo ngokuvamile asetshenziselwa ukusonga nokwenza izendlalelo ezicebile nge-resin ikakhulukazi ezisetshenziselwa imikhiqizo, okuhlanganisa izingqimba zomugqa wangaphakathi kanye nezingqimba zangaphandle. Izidingo ze-glass fibre mat enqubweni yokusonta zifana ngokuyisisekelo nalezo ezisendleleni yokubeka isandla.
I-5.Centrifugal casting molding: i-strand mat eqoshiwe ivame ukusetshenziswa njengempahla eluhlaza. I-strand mat eqoshiwe ibekwe ngaphambili ekubunjweni, bese i-resin yengezwa emgodini ojikelezayo wesikhunta, futhi amabhamuza omoya akhishwa nge-centrifugation ukwenza umkhiqizo uminyene. Ishidi le-mat liyadingeka ukuze libe nezici zokungena kalula kanye nokungena kahle komoya.
Omata bethu be-fiberglass bayizinhlobo eziningana: omati be-fiberglass surface,amacansi e-fiberglass aqoshiwe, kanye nomata be-fiberglass abaqhubekayo. I-strand mat eqoshiwe ihlukaniswe ibe yi-emulsion kanyei-powder glass fiber mats.
E-Glass Chopped Strand Mat Emulsion | |||||
Inkomba Yekhwalithi-1040 | |||||
225G | 300G | 450G | |||
Into yokuhlola | Umbandela Ngokusho | Iyunithi | Okujwayelekile | Okujwayelekile | Okujwayelekile |
UHLOBO LEGALASI | I-G/T 17470-2007 | % | R2O<0.8% | R2O<0.8% | R2O<0.8% |
I-AGENSI YOKUXHUMANA | I-G/T 17470-2007 | % | SILANE | SILANE | SILANE |
Isisindo Sendawo | I-GB/T 9914.3 | g/m2 | 225±45 | 300±60 | 450±90 |
Okuqukethwe kwe-Loi | I-GB/T 9914.2 | % | 1.5-12 | 1.5-8.5 | 1.5-8.5 |
I-CD Yamandla Amandla | I-GB/T 6006.2 | N | ≥40 | ≥40 | ≥40 |
Tension Amandla MD | I-GB/T 6006.2 | N | ≥40 | ≥40 | ≥40 |
Okuqukethwe Amanzi | I-GB/T 9914.1 | % | ≤0.5 | ≤0.5 | ≤0.5 |
I-Permeation Rate | I-G/T 17470 | s | <250 | <250 | <250 |
Ububanzi | I-G/T 17470 | mm | ±5 | ±5 | ±5 |
Amandla okugoba | I-G/T 17470 | I-MPa | Okujwayelekile ≧123 | Okujwayelekile ≧123 | Okujwayelekile ≧123 |
Imanzi ≧103 | Imanzi ≧103 | Imanzi ≧103 | |||
Isimo sokuhlola | |||||
I-Ambient Temperature(℃) | 10 | Umswakamo we-Ambient(%) |
Sinezinhlobo eziningi ze-fiberglass roving:ukuzulazula kwephaneli,fafaza uzulazule,Ukuzulazula kwe-SMC,ukuzulazula okuqondile,c ukuzulazula kwengilazi, kanye ne-fiberglass roving for chopping.Izilinganiso ezisheshayo nezinhle kakhulu, abeluleki abanolwazi ukuze bakusize ukhethe umkhiqizo ofanele ovumelana nazo zonke izimfuneko zakho, isikhathi esifushane sokukhiqiza, ukuphathwa kwekhwalithi ephezulu okunomthwalo wemfanelo, kanye nezinsizakalo ezihlukile zokukhokha nezokuthutha zamanani ashibhile Strand Chopped. I-Baking Needle 450 Tissue Roll Stitched E-Glass Machine E-Glass Chop Product Line 300g Silicon ye-Fiberglass Mat, Sithumele emazweni nasezifundeni ezingaphezu kuka-40, ezizuze ukuthandwa okuphezulu kubathengi bethu yonke indawo emhlabeni wonke.
Intengo Eshibhe Kakhulu I-China Fiberglass Mat kanye ne-Fiberglass Chopped Strand Mat, Eminyakeni eyi-11, siye sabamba iqhaza emibukisweni engaphezu kuka-20, sithola ukunconywa okuphezulu kakhulu kukhasimende ngalinye. Inkampani yethu ihlale ihlose ukuletha ikhasimende imikhiqizo engcono kakhulu ngentengo ephansi. Besenza imizamo emikhulu yokufeza lesi simo esiwinayo futhi sikwamukela ngobuqotho ukuthi uhlanganyele nathi. Hlanganyela nathi, futhi ubonise ubuhle bakho. Sizohlala siyisinqumo sakho sokuqala. Sithembe, awusoze waphelelwa yinhliziyo.