I-Resin ye-Polyester engagcwaliyo ye-Frp

incazelo emfushane:

I-resin engu-189 iyi-resin ye-polyester engagcwalisiwe ene-benzene tincture, i-cis tincture kanye ne-glycol ejwayelekile njengezinto eziyinhloko zokusetshenziswa. Incibilikiswe ku-styrene cross-linking monomer futhi ine-viscosity ephakathi nendawo kanye ne-medium reactivity.


Imininingwane Yomkhiqizo

Amathegi Omkhiqizo


IMPAHLA

•I-resin engu-189 ihlangabezana nezidingo zesitifiketi se-China Classification Society (CCS).
•Inezinzuzo zokuba namandla amahle nokuqina kanye nokuphola okusheshayo.

ISICELO

•Kufanelekela ubuciko bokubeka ngezandla ukwenza imikhiqizo ehlukahlukene engangeni manzi njengemikhumbi yepulasitiki eqiniswe ngefayibha yengilazi yangaphakathi, izingxenye zezimoto, imibhoshongo yokupholisa, amasinki, njll.

IKHWALITHI ELIYINHLOBO

 ITEM  Ibanga  Iyunithi Indlela Yokuhlola

Ukubukeka

Ophuzi okhanyayo
Ubumuncu 19-25 mgKOH/g I-GB/T 2895-2008

Ukuthamba, cps 25℃

0. 3-0. 6 Pa.s I-GB/T 2895-2008

Isikhathi sejeli, ubuncane obungu-25℃

12-30 umzuzu I-GB/T 2895-2008

Okuqukethwe okuqinile, %

59-66 % I-GB/T 2895-2008

Ukuqina kokushisa,

80℃

≥24 h I-GB/T 2895-2008

Amathiphu: Ukutholwa Kwesikhathi Sokuhlanzwa Kwegazi: 25°C amanzi okugeza, 50g i-resin ene-0.9g T-8m (NewSolar, L % CO) kanye ne-0.9g M-50 (Akzo-Nobel)

IMEMO: Uma unezidingo ezikhethekile zezici zokwelapha, sicela uxhumane nesikhungo sethu sobuchwepheshe

IMPAHLA YOMKHANIKI YE-CASTING

ITEM  Ibanga

 

Iyunithi

 

Indlela Yokuhlola

Ubulukhuni beBarcol

42

I-GB/T 3854-2005

Ukuhlanekezelwa Kokushisatumbuso

60

°C

I-GB/T 1634-2004

Ukwelula ngesikhathi sokuphumula

2.2

%

I-GB/T 2567-2008

Amandla okudonsa

60

I-MPa

I-GB/T 2567-2008

Imodulus yokudonsa

3800

I-MPa

I-GB/T 2567-2008

Amandla Okugobeka

110

I-MPa

I-GB/T 2567-2008

Imodulus eguquguqukayo

3800

I-MPa

I-GB/T 2567-2008

IMEMO: Idatha ebhalwe ohlwini iyimpahla evamile ebonakalayo, akufanele ihunyushwe njengokucaciswa komkhiqizo.

IMPAHLA YE-FRP

ITEM Ibanga

Iyunithi

Indlela Yokuhlola

Ubulukhuni beBarcol

64

I-GB/T 3584-2005

Amandla okudonsa

300

I-MPa

I-GB/T 1449-2005

Imodulus yokudonsa

16500

I-MPa

I-GB/T 1449-2005

Amandla Okugobeka

320

I-MPa

GB/T 1447-2005

Imodulus eguquguqukayo

15500

I-MPa

GB/T 1447-2005

IMYALELO

• I-resin engu-189 iqukethe i-wax, ayinazo izisheshisi kanye nezithasiselo ze-thixotropic.
• Kunconywa ukukhetha ama-resin ochungechunge lwe-/IO Peng Liu? Ortho-phthalic 9365 anezidingo zokusebenza eziphakeme.

 

UKUPAKISHA NOKUGCINA

• Umkhiqizo kufanele upakishwe esitsheni esihlanzekile, esomile, esiphephile nesivaliwe, isisindo esiphelele esingu-220 kg.
• Isikhathi sokuphila eshalofini: izinyanga eziyi-6 ngaphansi kwama-25℃, sigcinwe endaweni epholile futhi ehlanzekile
indawo enomoya.
• Noma yisiphi isidingo sokupakisha esikhethekile, sicela uxhumane nethimba lethu lokusekela

QAPHELA

• Lonke ulwazi olukulolu hlu lusekelwe ezivivinyweni ezijwayelekile ze-GB/T8237-2005, ukuze lubhekiselwe kuphela; mhlawumbe luhluke kudatha yangempela yokuhlolwa.
• Enqubweni yokukhiqiza yokusebenzisa imikhiqizo ye-resin, ngoba ukusebenza kwemikhiqizo yomsebenzisi kuthintwa yizici eziningi, kubalulekile ukuthi abasebenzisi bazihlole ngaphambi kokukhetha nokusebenzisa imikhiqizo ye-resin.
• Ama-resin e-polyester angagcwele awazinzile futhi kufanele agcinwe ngaphansi kwama-25°C emthunzini opholile, ahanjiswe emotweni efrijini noma ebusuku, egwema ukukhanya kwelanga.
• Noma yisiphi isimo esingafanele sokugcina nokuthutha impahla sizobangela ukufinyezwa kokuphila kwayo eshalofini.